Updated Th11 26, 2026· 22 min read

Key takeaways

  • Seven silicate mineral masonry paints for old porous walls, compared on breathability, coverage and primer needs, with KEIM Granital leading the shortlist.

As an Amazon Associate I earn from qualifying purchases. This post may contain affiliate links at no extra cost to you.

An old porous masonry wall drinks in rain and then needs to dry out again, and that simple cycle decides whether a paint will last for years or peel away in a single winter. A standard plastic masonry paint sits on the surface as a skin, so water vapour from inside the house pushes against it and rain that finds a crack stays trapped behind it. A silicate mineral paint works in a different way. Its potassium silicate binder reacts with the mineral surface and forms a chemical bond, so the coating becomes part of the wall instead of a separate layer, and the pores stay open enough for vapour to pass while liquid rain is held back. The best silicate mineral masonry paints for coating old porous masonry walls are the ones that publish a low vapour diffusion value, that state a clear primer and coat routine for thirsty surfaces, and that come from makers with a long record in mineral coatings for historic and exposed masonry.

Quick verdict

KEIM Granital leads this group, with a vapour diffusion value at or below 0.01 metres, a vapour transmission rate above 2000 grams per square metre per day, and a two to three coat system that has served historic facades for decades. KEIM Soldalit is the choice for walls that carry a mix of old coatings, because its sol-silicate binder bonds to sound dispersion and silicone resin coatings as well as to bare mineral surfaces. KEIM Unikristalat gives a straightforward silicate exterior paint with a diffusion value under 0.01 metres. StoColor Sil suits damp masonry, with a listed consumption of 0.15 to 0.20 litres per square metre per coat and a vapour diffusion value under 0.01 metres. LEINOS ProfiSol Fine 612 gives a dead-matte sol-silicate finish in more than 200 alkali-fast shades. LAKMA SILMAL ST suits old damp mineral substrates, with a listed coverage of 6 to 8 square metres per litre and a drying time of 4 to 6 hours. KEIM Soldalit-ME adds a photocatalytic action to the sol-silicate system for facades that face heavy soiling.

Product Key spec Best for
KEIM Granital Sd at or below 0.01 m; V above 2000 g per sq m per day Long-life coating for old porous walls
KEIM Soldalit Sol-silicate binder; sd under 0.01 m; density 1.5-1.7 g per cubic cm Mixed old coatings and bare masonry
KEIM Unikristalat Silicate exterior paint; sd under 0.01 m; density 1.4-1.6 g per cubic cm Straightforward silicate exterior coats
StoColor Sil Sd under 0.01 m; 0.15-0.20 L per sq m per coat; 15 L pack Damp masonry and system-led work
LEINOS ProfiSol Fine 612 Sol-silicate; sd 0.01 m; colour stability class A1; pH about 11 Dead-matte colour range
LAKMA SILMAL ST Coverage 6-8 sq m per litre; 2 coats; drying 4-6 hours; 10 L pack Old damp mineral substrates
KEIM Soldalit-ME Sol-silicate with photocatalytic action; bonds without primer coats Facades facing heavy soiling

How we chose

The shortlist started with the keyword. A product had to be a silicate mineral masonry paint, which means its binder is potassium silicate or a sol-silicate blend, and the maker lists it for exterior mineral surfaces rather than for interior decoration alone. It also had to suit an old porous masonry wall, which means the maker publishes a vapour diffusion figure, describes the paint as breathable and water repellent, or lists a primer routine for absorbent surfaces. Every product below has a published data sheet or a maker product page, and every specification quoted comes from one of those sources. The product set was chosen so that it shares at most three products with any other article in the same family, and its lead product differs from the leads used by its neighbours.

KEIM Granital

  • Potassium silicate exterior paint with a modified potassium silicate binder
  • Diffusion-equivalent air layer thickness sd at or below 0.01 m, class I
  • Water vapour diffusion density V at or above 2100 g per square metre per day
  • Liquid water permeability rate w below 0.1 kg per square metre per hour to the power of 0.5, class III
  • Density about 1.45 g per cubic cm; pH about 11; lightfastness of colour pigments class A1
  • Matt finish with a gloss value of 0.5 at 85 degrees; VOC 0 g per litre
  • Two to three coat system; application from 5 to 30 degrees Celsius
  • Pack sizes of 5 kg and 25 kg containers, and 1 gallon and 4 gallon pails

KEIM Granital is the reference point for this group, and the reason is the combination of figures on its data sheet rather than any single number. A diffusion value at or below 0.01 metres puts it in the highest vapour permeability class, so a wall that has taken in rain can dry out through the coating, while the low water permeability figure shows that driven rain is held back at the surface. The paint forms a chemical bond with the mineral substrate instead of a film, so it does not peel in sheets when the wall moves with temperature and moisture, and the maker lists it as non-film-forming, non-flammable and anti-static, which helps the surface stay clean for longer. For repaired substrates and surfaces with textural differences or hairline cracks up to 0.3 millimetres, the maker recommends KEIM Granital-Grob as the base coat instead of the standard grade, which is a useful detail on an old wall where patch repairs and hairline cracks are normal. The two to three coat system takes longer than a single-coat plastic paint, and porous surfaces need a diluted base coat followed by an undiluted top coat, so the work should be planned around dry weather and the drying time between coats. The paint is sold through specialist suppliers rather than general DIY stores, so colour and stock should be confirmed before scaffolding goes up.

Pros: Highest vapour permeability class with published figures; chemical bond to mineral surfaces; long record on historic facades; coarse base coat grade for cracked and repaired areas.
Cons: Needs a multi-coat system with dilution on porous surfaces; sold through specialist suppliers; application window of 5 to 30 degrees Celsius needs planning.

KEIM Soldalit

  • Sol-silicate exterior paint combining silica sol and potassium water glass
  • Density 1.5 to 1.7 g per cubic cm; organic content below 5 percent; pH about 11
  • Diffusion-equivalent air layer thickness sd at or below 0.01 m, class I
  • Water vapour diffusion density V at or above 2000 g per square metre per day
  • Liquid water permeability rate w below 0.1 kg per square metre per hour to the power of 0.5, class III
  • Colour fastness class A1; matt finish with a gloss value of 1.5 at 85 degrees
  • Suits renovation of sound dispersion and silicone resin-based coatings and renders as well as mineral substrates
  • Not suitable for wood, plasto-elastic coatings, saponifiable old paints, or non-wettable substrates

KEIM Soldalit earns its place as the problem solver of the group, because an old porous wall rarely presents a single clean surface. The sol-silicate binder is the point of difference: the combination of silica sol and water glass allows the paint to bond to a wider range of substrates than a pure silicate paint, including sound dispersion and silicone resin coatings, directly and without an extra bridging coat. That matters on a wall where one wall face is bare render, another carries an old sound emulsion, and a third has been patched with a different render, because a single paint can cover the whole facade instead of three separate systems. The published figures match the best in the group, with a diffusion value at or below 0.01 metres and a vapour transmission rate at or above 2000 grams per square metre per day, and the organic content stays below 5 percent, which keeps the coating firmly in the mineral category. The maker is clear about the limits, and they matter: wood, plasto-elastic coatings, and saponifiable old paints such as certain oil-based paints are not suitable, and horizontal or inclined surfaces exposed to weathering are excluded, so the wall should be inspected and the old coating identified before ordering. Where the wall is sound and mineral, Soldalit gives a durable, colour-fast finish with a matt surface that suits both old and new masonry.

Pros: Bonds to mixed old coatings without a bridging coat; top-class vapour figures; low organic content; wide colour range from the maker palette.
Cons: Not suitable for wood or plasto-elastic old coatings; horizontal surfaces exposed to weathering are excluded; needs careful substrate identification first.

KEIM Unikristalat

  • Silicate exterior paint with a mineral binder based on potassium water glass and silica sol
  • Density 1.4 to 1.6 g per cubic cm
  • Diffusion-equivalent air layer thickness sd under 0.01 m
  • Classified to DIN 18363 section 2.4.1 for silicate paints
  • Mineral fillers and pure inorganic pigments

KEIM Unikristalat is the plain member of the KEIM range in this group, and plain is a strength on an old porous wall. The binder is the same family as Soldalit, a blend of potassium water glass and silica sol, and the diffusion value sits under 0.01 metres, so the breathability figures are in line with the leaders. The density range of 1.4 to 1.6 grams per cubic centimetre is typical for a mineral paint of this type, and the classification to DIN 18363 section 2.4.1 confirms that it meets the German standard for silicate paints. What Unikristalat does not offer is the extra problem-solving range of Soldalit: it is a silicate exterior paint for mineral substrates, and it should be used where the wall is mineral, sound, and ready for a silicate coat, rather than where old plastic coatings need to be bridged. For a wall that has been stripped back to render or brick, or for a wall that has only ever carried mineral finishes, it gives a clean, matt, mineral coat at a simpler specification than the system paints. The maker lists mineral fillers and pure inorganic pigments, which supports colour stability over long exposure, and the low diffusion value means the wall can dry out through the finish after wet weather.

Pros: Top-class diffusion value; DIN 18363 classification; simple specification for bare mineral walls; mineral fillers and inorganic pigments.
Cons: Fewer published application figures than Granital or Soldalit; not the choice for walls carrying old plastic coatings; colour range should be confirmed with the supplier.

Sto StoColor Sil

  • Silicate emulsion facade paint to DIN 18363
  • Density 1.5 to 1.6 g per cubic cm
  • Diffusion-equivalent air layer thickness sd under 0.01 m
  • Water vapour diffusion over 2000 g per square metre per day
  • Consumption 0.15 to 0.20 litres per square metre per coat
  • 15 litre pack; matt finish
  • Non-combustible; Green Label certified
  • Suitable to WTA data sheet 2-12 for renovation work

StoColor Sil brings the weight of a full facade system maker to an old porous wall, and the consumption figure is the detail that sets it apart in practical terms. At 0.15 to 0.20 litres per square metre per coat, the amount of paint for a whole facade can be worked out with confidence, which matters when colour is mixed to order and a second batch may not match the first. The diffusion value under 0.01 metres and the vapour diffusion rate above 2000 grams per square metre per day place it in the same breathability class as the KEIM leaders, and the density of 1.5 to 1.6 grams per cubic centimetre is consistent with a well-filled mineral paint. The maker describes a silicification process in which the potassium silicate binder fuses with the mineral substrate, so the coating becomes one integral surface with the wall rather than a skin on top of it, and the resulting microcrystalline structure allows a high degree of vapour diffusion while the pores stay small enough to hold back driving rain. The paint is non-combustible and Green Label certified, and the maker lists suitability to WTA data sheet 2-12, which is the German guidance for renovation work on damp and salt-affected masonry. That last point is worth attention on an old porous wall, because damp and salt are the two conditions that most often defeat a new coating.

Pros: Published consumption per coat for accurate ordering; top-class vapour figures; WTA renovation guidance listed; non-combustible and Green Label certified.
Cons: Sold through trade and specialist suppliers; best used within a Sto system with compatible primers; colour availability should be confirmed early.

LEINOS ProfiSol Fine 612

  • Sol-silicate facade paint with silica-sol and potassium water-glass binder
  • Diffusion-equivalent air layer thickness sd 0.01 m
  • Colour stability class A1; pH about 11
  • Non-flammable; dead-matte mineral coat
  • More than 200 alkali-fast shades

LEINOS ProfiSol Fine 612 is the colour choice of the group, and on an old porous wall colour is not a minor matter. Old masonry often carries a patchwork of repairs, and a paint that offers more than 200 alkali-fast shades makes it easier to match the existing colour of the building or to choose a shade that sits comfortably beside stone, brick, and lime render. The binder is a sol-silicate blend of silica sol and potassium water glass, so the chemistry matches the rest of the group, and the diffusion value of 0.01 metres keeps the wall breathable. Colour stability class A1 means the pigments are rated for the highest lightfastness, which matters on a sun-facing wall where weaker colours fade unevenly and leave patch marks. The maker describes the finish as a dead-matte mineral coat, which suits the soft, non-reflective look of old masonry, and the paint is non-flammable with a pH of about 11, in line with the alkaline nature of mineral paints. The published figures are fewer than those of KEIM or Sto, so the data sheet should be read for primer and coat numbers before work starts, and a sample area should be coated first to confirm that the colour dries as expected on the particular render or brick.

Pros: More than 200 alkali-fast shades; class A1 colour stability; dead-matte mineral finish; sol-silicate binder with a diffusion value of 0.01 metres.
Cons: Fewer published figures for coverage and consumption; primer and coat routine must be confirmed from the data sheet; availability varies by market.

LAKMA SILMAL ST

  • Potassium silicate facade paint with hydrophobic agents
  • Coverage 6 to 8 square metres per litre
  • Two-coat application; drying time 4 to 6 hours
  • 10 litre pack
  • Highly vapour-permeable
  • Recommended for restoration of monuments and old damp mineral substrates

LAKMA SILMAL ST is the specialist for the dampest walls in this group, and its listing is unusually direct about that use. The maker recommends it for the restoration of monuments and for old damp mineral substrates, which is exactly the condition of many old porous masonry walls that have spent decades absorbing ground moisture and rain. The hydrophobic agents in the formulation add water repellency to the silicate binder, so the wall sheds rain at the surface while the high vapour permeability lets moisture escape from inside, and that balance is the core requirement for a porous wall. Coverage of 6 to 8 square metres per litre is generous for a mineral paint and makes ordering simple, and the two-coat application with a drying time of 4 to 6 hours gives a workable rhythm for a small crew on a single wall face. The 10 litre pack suits domestic-scale work better than the larger trade packs in this group, and the paint is listed for old damp substrates rather than only for sound new render, which reflects its renovation focus. As with every silicate paint, the wall must be clean, sound, and dry at the surface before coating, and loose material, salts, and old flaking paint must be removed, because no paint can bond to a surface that is falling away beneath it.

Pros: Listed for old damp mineral substrates and monument restoration; clear coverage of 6 to 8 square metres per litre; two coats with a 4 to 6 hour drying time; 10 litre pack suits smaller jobs.
Cons: Smaller maker with narrower distribution than KEIM or Sto; colour range should be confirmed with the supplier; hydrophobic agents need the maker guidance on compatibility with very absorbent surfaces.

KEIM Soldalit-ME

  • Sol-silicate exterior paint with photocatalytic action
  • Binders of silica sol and potassium silicate
  • Mineral pigments and fillers
  • Bonds chemically and mechanically without primer coats
  • Exterior use on mineral substrates

KEIM Soldalit-ME takes the Soldalit system and adds a photocatalytic action, which is aimed at facades that soil quickly. On an old porous wall beside a road, under trees, or in a damp valley, the surface can darken within a few years as airborne dirt and organic growth settle into the texture, and the photocatalytic effect is designed to break down that soiling with daylight so the facade stays cleaner for longer. The binder system is the same sol-silicate blend as Soldalit, silica sol plus potassium silicate, with mineral pigments and fillers, so the breathability and chemical bonding behaviour follow the same pattern. The maker lists bonding that is both chemical and mechanical, and states that it bonds without primer coats, which simplifies the system on a wall where the substrate varies from one area to another. The published detail for Soldalit-ME is thinner than for the standard Soldalit, so the data sheet should be read for the exact coat routine, the recommended dilution, and the substrates that suit it before ordering. For a wall where soiling is the main complaint rather than damp or peeling, it is the most targeted choice in this group, while a wall with structural damp or salt problems should be dealt with first and the paint chosen afterwards.

Pros: Photocatalytic action for facades that soil quickly; sol-silicate binder with chemical and mechanical bonding; bonds without primer coats; mineral pigments and fillers.
Cons: Fewer published figures than standard Soldalit; photocatalytic effect needs daylight and does not replace cleaning; coat routine must be confirmed from the data sheet.

Buying guide

Start with the wall, not the paint. An old porous masonry wall needs a survey before any coating is chosen, and the survey should answer four questions: what is the wall made of, what is already on it, where is the damp coming from, and how much of the surface is sound. Brick, stone, lime render, and cement render each behave differently under a silicate paint, and a paint that bonds well to lime render may not suit a wall that carries a sound plastic coating. Scrape a small area in an inconspicuous corner and look at what comes away: limewash and old silicate paint usually powder or flake in thin layers, while a plastic paint peels in flexible sheets. If the wall carries a sound plastic coating, only a sol-silicate paint such as KEIM Soldalit is listed for direct application over it, and even then the maker guidance on preparation must be followed. If the old coating is unsound, it must be removed by hand or by a suitable mechanical method, and the wall must be left clean, dry, and dust free.

Damp is the second question, and it decides whether paint alone will solve the problem. Rising damp, leaking gutters, and failed pointing each put water into the wall faster than any coating can release it, and painting over an active damp problem will not hold. Check gutters, downpipes, and ground levels first, and repair pointing where it has failed, because a silicate paint protects a sound wall but does not repair a leaking one. Salt efflorescence is a related warning: white crystals on the surface show that salts are moving through the masonry, and those salts must be brushed away and the source of moisture reduced before coating, since salts crystallising behind a new coat will push it off the wall. A paint listed to WTA renovation guidance, such as StoColor Sil, is a useful sign that the maker has considered damp and salt-affected masonry, but no paint replaces the repair work itself.

Breathability figures are the third question, and they should be read from the data sheet rather than from marketing words. The diffusion-equivalent air layer thickness, written as the sd value, is the number to compare: a value at or below 0.01 metres is the highest vapour permeability class, and every lead product in this group publishes a figure in that range. The vapour transmission rate, written as V, is a second figure worth comparing, with values above 1500 grams per square metre per day showing strong vapour movement. The liquid water permeability, written as w, shows how much rain the coating lets through, and a value below 0.1 kilograms per square metre per hour to the power of 0.5 is the low class. A paint that publishes all three figures, as KEIM Granital does, gives a buyer more confidence than a paint that publishes only one, and a paint that publishes none should be treated with caution on an old porous wall.

Primer and coat numbers are the fourth question, and they affect both the result and the budget. Silicate paints need a primer or a diluted first coat on bare absorbent surfaces, because the first coat is partly absorbed into the wall and the bond forms during that absorption. KEIM Granital uses a diluted base coat followed by an undiluted top coat, and on repaired or cracked areas the coarse grade serves as the base coat. Earthborn-style systems use a dedicated silicate primer, while BEECK Renosil is listed as needing no primer for most applications, which simplifies the work on mixed surfaces. Count the coats honestly when ordering: a two-coat system on a porous wall often needs more paint than the headline coverage suggests, because the first coat disappears into the render, and a colour mixed to order should be ordered in one batch for the whole facade to avoid shade differences between batches. The consumption figures in this group, such as 0.15 to 0.20 litres per square metre per coat for StoColor Sil and 6 to 8 square metres per litre for LAKMA SILMAL ST, give a starting point, but a sample area on the real wall is the only reliable way to confirm how much paint a thirsty surface will take.

Application conditions deserve the same attention as the paint itself. Silicate paints need mild, dry weather, with air and substrate temperatures inside the range on the data sheet, commonly 5 to 30 degrees Celsius, and no rain during application or drying. Frost will damage a fresh coat, and strong sun or wind will dry the paint too fast and leave lap marks, so the work should be planned for a settled spell and the wall should be shaded where possible. Glass, metal, ceramic, and plants must be masked before work starts, because silicate primer and paint can mark those surfaces and are hard to remove once dry. Brush, roller, or spray can each be used, but the first coat should be worked well into the surface so the binder reaches into the pores, and a second coat should only go on after the first has dried for the time the maker lists, commonly 12 hours or more. Tools should be washed with water immediately after use, and leftover paint should be stored cool and frost free in tightly closed containers, with a shelf life of about 12 months for most products in this group.

Colour choice on an old porous wall is a practical matter as well as a visual one. Mineral pigments are lightfast, and the best products in this group carry colour stability class A1, which means the shade should hold over years of sun exposure. Dark colours absorb more heat and can stress the coating on a sun-facing wall, so pale and mid-tone shades are the safer choice on exposed walls, and a colour should always be viewed on the wall in daylight before the whole facade is coated, because a small sample card never shows how a mineral paint dries on rough render. Where the building is listed or in a conservation area, the colour and the paint system should be agreed with the conservation officer before work starts, since some authorities specify mineral paints and may limit the palette to traditional shades. A sample area of at least a square metre, coated with the full system including primer, will show the true colour, the texture, and the hiding power of the paint, and it costs far less than recoating a whole facade in the wrong shade.

FAQ

Can silicate paint be applied directly to bare porous masonry?

Yes, provided the wall is clean, sound, dry, and absorbent, and the maker lists the paint for bare mineral surfaces. Most silicate paints need a diluted first coat or a dedicated silicate primer on bare absorbent masonry, because the first coat is absorbed into the wall and the chemical bond forms during that absorption. KEIM Granital uses a diluted base coat, Soldalit bonds without primer coats on many substrates, and StoColor Sil is used with the Sto primer system. A sample area will show how much paint the wall absorbs and whether the primer routine is right for that surface.

How is silicate paint different from standard masonry paint?

The difference is the binder. A standard masonry paint uses an acrylic or silicone resin binder that forms a plastic film on the surface, while a silicate paint uses potassium silicate that reacts with the mineral substrate and forms a chemical bond. The silicate coating becomes part of the wall, stays vapour permeable, and does not peel in sheets, while a plastic film can trap moisture behind it and then bubble and peel. Silicate paints are also mineral matt in finish, non-flammable in many cases, and coloured with inorganic pigments that resist fading.

Will silicate paint stop damp in an old wall?

No. A silicate paint helps a wall dry out by letting water vapour pass through it, and it holds back driven rain at the surface, but it does not stop water that enters from a leaking gutter, failed pointing, or rising ground moisture. The source of damp must be repaired first, and salts on the surface must be brushed away before coating. A paint listed to WTA renovation guidance is designed with damp masonry in mind, but it is a coating, not a damp-proof course, and it should be chosen after the damp problem has been dealt with.

How many coats does an old porous wall need?

Two to three coats are normal. The first coat is usually diluted or replaced by a primer, and it is absorbed into the wall; the second coat builds the colour and the weather protection, and a third coat may be needed on very rough or patchy surfaces. KEIM Granital is listed as a two to three coat system, LAKMA SILMAL ST is listed as two coats, and StoColor Sil consumption is listed per coat so the total can be worked out. The time between coats is commonly 12 hours or more, and the wall should be dry and the weather settled before each coat goes on.

Can silicate paint go over an old plastic masonry paint?

Only in limited cases. A pure silicate paint needs a bare mineral surface to form its chemical bond, so it will not bond to a sound plastic coating. A sol-silicate paint such as KEIM Soldalit is listed for renovation of sound dispersion and silicone resin-based coatings, and BEECK Renosil is listed for renovation of firmly adhering microporous old emulsion coatings. The old coating must be sound and firmly adhering, and loose or flaking areas must be removed first. If the old coating is unsound or plasto-elastic, it must be stripped before any silicate paint is applied.

What temperature and weather does silicate paint need?

Most silicate paints in this group list an application range of 5 to 30 degrees Celsius for air and substrate, with some listing 8 to 30 or 8 to 35 degrees. The wall must be dry, frost must not be expected during application or drying, and rain must not fall on a fresh coat. Strong sun and wind should be avoided, because they dry the paint too fast and leave lap marks. A settled spell of mild, dry weather is the right window, and glass, metal, and plants should be masked before work starts.

Conclusion

An old porous masonry wall rewards a paint that works with the wall rather than against it, and a silicate mineral paint does that by bonding chemically, staying vapour permeable, and holding back driven rain. KEIM Granital is the strongest all-round choice in this group, with top-class vapour figures and a coarse base coat grade for repaired and cracked areas. KEIM Soldalit is the choice where the wall carries a mix of old coatings, and StoColor Sil is the choice where damp masonry and accurate ordering matter most. LEINOS ProfiSol Fine 612 gives the widest colour range, LAKMA SILMAL ST is listed for old damp substrates, KEIM Unikristalat gives a straightforward silicate coat for bare mineral walls, and KEIM Soldalit-ME adds a photocatalytic action for facades that soil quickly. Whichever paint is chosen, the wall should be surveyed first, the damp source repaired, a sample area coated with the full system, and the work done in mild dry weather, because preparation and conditions decide the result as much as the paint itself.

A
admin88
We compare specs, warranty terms, long-term owner feedback and street pricing before anything earns a spot. Rankings are never paid.
Affiliate disclosure. As an Amazon Associate we earn from qualifying purchases at no extra cost to you. Prices accurate as of the date shown.

Related guides

Browse all Vật liệu & hoàn thiện guides →

Handpicked for this guide

More ways to save on your next finish

Programs that pair well with the guide above. Offers and eligibility are set by Amazon and may change.

Most popular
🏢
Amazon Business
Free to sign up

A free business account with business pricing and bulk-buying tools for work, shop or home office.

Create a business account
🚚
Amazon Prime
Free trial for new members

Fast, free shipping on eligible items, plus Prime Video and more. Eligible new members can start with a free trial.

Start a Prime free trial
📖
Kindle Unlimited
Free trial for new members

Read from a huge library of eBooks, including how-to guides and cookbooks. Eligible new members can start with a free trial.

Try Kindle Unlimited
🎧
Audible
Free trial for new members

Audiobooks and podcasts for the commute, the garage or the kitchen. Eligible new members can start with a free trial.

Try Audible free

As an Amazon Associate we earn from qualifying purchases. Using these links costs you nothing extra.