A sand finished exterior wall hides small damage well from a distance, and that is exactly why a careless patch stands out so clearly up close. The finish is a uniform field of fine grit, and the eye reads any change in grain size, direction, or flatness as a scar. How to repair textured stucco patches on a sand finished exterior wall is therefore less about filling a hole and more about rebuilding the wall in the same layers the original plasterer used, then finishing the surface with the same motion and the same aggregate size. When the coats go back in the right order and the finish coat carries the same sand, the patch can sit quietly beside old work that has weathered for years.

Sand finish stucco earns its name from the fine silica aggregate in the finish coat. The grains show at the surface and give the wall a soft, even sparkle in low sun. Because the texture is shallow and regular, a patch that is too smooth looks like a bald spot, while a patch that is too rough looks like a scab. The good news is that the finish is one of the most forgiving textures to copy, provided the base coats are flat and the finish coat is floated with a sponge or rubber float in the same circular motion used on the rest of the wall. A sample panel on a scrap board is the place to settle the mix and the motion before the trowel ever touches the wall.

This guide walks through the full repair on a flat exterior wall: reading the damage, cutting back to sound material, rebuilding the scratch and brown coats, and floating a sand finish that matches the grain around it. The products named here are real materials with published data sheets, and the numbers quoted come from those sheets. Where a detail depends on the wall in front of you, the guide says so rather than guessing.

Quick answer

Cut the damaged stucco back to sound material, undercut the edges slightly, dampen the area, and rebuild in coats no thicker than 3/8 inch each: a scored scratch coat, a level brown coat, and a thin sand finish coat floated with a sponge float. A premixed acrylic patch such as Quikrete Stucco Patch No. 8650 suits shallow surface damage up to 1/4 inch deep, while deeper holes need a cement-based patch such as Rapid Set Stucco Patch, applied in layers with curing time between coats. Match the sand grain by using a patch material with a fine aggregate in the same size range as the existing finish, and practice the float motion on a sample panel first so the grain pattern lands the same way on the wall. Keep the patch damp while it sets, protect it from rain and hot sun, and allow the full cure time before painting.

Item What it does When to use it
Quikrete Stucco Patch No. 8650 Premixed acrylic patch that fills shallow defects and blends with sand texture Surface chips, hairline cracks, and shallow patches up to 1/4 inch deep
Rapid Set Stucco Patch Fast-setting cement patch for full-depth repair in one application Holes that reach the brown coat or lath, up to 1 inch thick
Marshalltown Sponge Float 12 x 5 in Floats the finish coat into a uniform sand grain Final floating of the sand finish and blending the patch edge
Marshalltown M38 Rubber Float Fine 9 x 4 in Fine-cell rubber float for a smooth, even top coat Fine sand finishes where a sponge leaves too much drag
Larsen Weld-Crete Bonding Agent Chemical bond between new stucco and sound old concrete or stucco Dense or slick substrates where a mechanical key alone is not enough
Marshalltown PermaShape Finishing Trowel 14 x 5 in Stainless finishing trowel with a pre-worn edge for flat, line-free work Laying on and levelling the brown coat and finish coat

Step by step

Step 1: Read the damage and the finish

Start by looking at the wall in raking light, with the sun low or a work light held at a shallow angle. Raking light shows every hollow, hump, and loose edge that flat daylight hides. Tap the stucco around the damage with a knuckle or the handle of a trowel. Sound stucco rings solid and dull; hollow stucco sounds drum-like and marks the edge of the area that has lost its bond. Mark the hollow area with chalk, then extend the mark about 2 inches beyond the damage in every direction, because a patch needs sound material all around it to grip.

Next, read the finish itself. Rub a fingertip across the sand finish and note the grain: fine sand finishes feel like coarse paper, with grains that catch the skin but do not snag it. Compare the grain at the top of the wall with the grain near the damage, since sun and rain wear the aggregate differently over the years. Look at the colour too, and accept that a fresh patch dries to a lighter tone than old stucco and darkens as it ages. A patch that matches in grain and sits flat will blend within a season; a patch that matches in colour on day one but sits proud of the wall will stay visible.

Check for water before any repair begins. Brown streaks, soft spots, bubbling paint, or a musty smell near the damage point to moisture behind the stucco. A patch laid over a wet wall traps water inside and fails from behind. Find the source first: a leaking gutter joint, a failed sealant line at a window, a sprinkler head aimed at the wall, or a missing drip edge. Fix the water problem, let the wall dry, and only then start the patch. If the stucco feels soft and crumbly deep into the wall, or if the damage covers a large area, the repair has moved beyond a patch and needs a plasterer.

Step 2: Cut back to sound stucco and shape the edges

Cutting back is the least pleasant part of the job and the most important. Use a cold chisel and a hammer to remove loose and hollow stucco, working from the centre of the damage outward to the chalk line. Keep the blows light and controlled; heavy swings crack sound stucco beyond the line and can tear the metal lath behind it. Where the stucco is still bonded but cracked, a diamond blade on an angle grinder cuts a clean line, but wear eye protection and a dust mask, and keep the blade shallow so it does not cut the lath.

Shape the edges of the opening with a slight undercut, so the opening is wider at the back than at the face. This dovetail shape locks the patch mechanically: the new material keys behind the old edge instead of sitting in a straight-sided hole that can pop out. Aim for a gentle slope rather than a sharp notch. Brush the opening clean with a stiff wire brush, then vacuum or blow out the dust. Any loose sand or powder left in the opening weakens the bond, because the patch grips the dust instead of the wall.

If the damage goes through to the metal lath, inspect the lath before going further. Sound galvanized lath that is still firmly fixed can stay. Rusted, torn, or loose lath must be cut out and replaced with a new piece of the same type, overlapped at least 2 inches over the old lath on all sides and fixed to the framing. The patch is only as strong as the base it hangs from, and a patch over failed lath cracks along the edge of the old work within months.

Step 3: Dampen the substrate and apply a bonding agent where needed

Stucco draws water out of fresh patch material fast, and a dry substrate can rob the patch of the moisture it needs to cure. Mist the opening and the surrounding stucco lightly with clean water from a spray bottle or a garden sprayer. The surface should look damp and darkened, not wet and running. On a hot day, mist the area twice, a few minutes apart, so the moisture soaks in rather than flashing off the surface.

On dense, smooth, or previously painted substrate, a bonding agent adds a chemical bridge where a mechanical key is hard to get. Larsen Weld-Crete is made for exactly this situation: the maker lists it for bonding new Portland cement plaster and stucco mixes to structurally sound concrete, and the coverage listed on the data sheet is 200 to 300 square feet per gallon. Brush or roll it on in a thin, even film and follow the maker guidance on waiting time before the patch goes on. Do not use a bonding agent as a substitute for cleaning the surface; dust, oil, and loose paint still have to come off first, because the agent bonds to whatever it touches, including dirt.

Where the substrate is open and rough, with a good mechanical key from the old scratch coat, dampening alone is often enough. The scratch coat of the original wall was scored on purpose to give the next coat something to grip, and the broken edge of the old brown coat gives the same grip. Judge the surface in front of you: if it feels slick or sealed, use the bonding agent; if it feels open and sandy, water alone will do.

Step 4: Mix the patch material to the right consistency

For shallow damage, a premixed patch is the simplest route. Quikrete Stucco Patch No. 8650 comes ready to use in a 1 quart pail, and the maker describes it as a sanded acrylic formula that blends with the texture of the surrounding stucco. Stir it well before use, and do not thin it with water unless the label allows it. The data sheet limits each layer to 1/4 inch thick, with 24 hours between layers for anything deeper, and the coverage listed is about 3.25 square feet at 1/8 inch thick. Skin forms in about 20 to 40 minutes, and the patch becomes hard in about 2 hours, with curing continuing for up to 3 days. Air and surface temperature must stay above 50 degrees Fahrenheit during application.

For deeper holes, a cement-based patch gives the repair its structure. Rapid Set Stucco Patch mixes with water at a ratio of 1 part water to 4 parts powder, or 2 quarts of water per 25 pound bag, and the data sheet lists a working time of about 20 minutes. It can be applied from 1/8 inch to 1 inch thick in a single application, and it can be primed and painted after about 2 hours. The sand in the mix is a number 16 to 20 silica sand, which is the size range the maker designs to match most existing stucco finish coats. Mix only as much as can be placed inside the working time, and never add water to a mix that has started to stiffen; retempering weakens the set and leads to a patch that powders at the surface.

Consistency matters more than any single ingredient. A scratch or brown coat mix should hold its shape on the trowel without slumping, and should spread under pressure without tearing. A finish coat mix for a sand finish is slightly wetter, so the float can move the aggregate without dragging it. Mix a small batch first and spread it on a sample panel: a piece of cement board or a scrap of plywood faced with lath. If the mix slides off the panel, it is too wet; if it tears and leaves bare spots, it is too dry.

Step 5: Build the scratch coat and score it

Press the first coat firmly into the opening with a trowel, forcing the material into the edges and against the lath. Work from the edges inward, squeezing the mix into the undercut so the patch locks behind the old stucco. This edge-first pass is the step that stops a crack from opening along the joint later. Once the edges are filled, fill the middle and level the coat to about 3/8 inch thick, leaving it below the face of the surrounding wall by the thickness of the coats still to come.

Score the scratch coat while it is still soft. Drag a notched trowel or a scarifier across the surface in horizontal lines, about 1/8 inch deep. The grooves give the brown coat a mechanical key, and horizontal scoring suits a vertical wall because it resists the downward pull of the next coat. Do not score so deeply that the grooves cut through to the lath.

Let the scratch coat cure moist. The trade guidance quoted in repair literature calls for moist curing of 48 to 72 hours before the next coat, and the coat should be solid but still able to receive the brown coat. Mist the surface lightly a few times a day in dry weather, and shade it from direct sun with a damp cloth or a piece of plywood stood off the wall. A scratch coat that dries too fast shrinks and cracks, and those cracks print through every coat above them.

Step 6: Apply the brown coat and level it flush

Dampen the scratch coat before the brown coat goes on, for the same reason as before: a dry base steals water from the fresh mix. Lay the brown coat on with the trowel, again pressing firmly at the edges first, and build it to about 3/8 inch thick. The brown coat should end up just below the face of the surrounding finish coat, leaving room for the thin finish layer. If the brown coat finishes level with the old finish, the final coat has nowhere to go and the patch ends up standing proud of the wall.

Level the brown coat with a straightedge or a darby, drawing it across the patch in slow, even passes. Check the level with a straight piece of timber laid across the patch and the old stucco on both sides; any rocking or gap shows a high or low spot. Float the brown coat with a wood or sponge float to close the surface, then leave it to cure. The brown coat needs the same moist curing as the scratch coat, and the same protection from sun and wind. A brown coat that is still green when the finish goes on will move as it dries and crack the finish.

Step 7: Float the sand finish to match the grain

The finish coat is thin, often about 1/8 inch, and it is where the match is won or lost. Dampen the brown coat lightly. Spread the finish mix over the patch with the trowel, keeping it inside the patch area and going right up to the old edge without spreading onto the old finish. A useful trick from trade practice is to tape the old finish at the edge of the patch, so the new finish stops exactly at the line and the tape peels away to leave a clean joint.

Let the finish stiffen slightly, then float it. A Marshalltown Sponge Float, 12 inches by 5 inches with a pad about 1-1/8 inches thick, is the tool for this finish: the sponge carries water, keeps the surface damp, and rolls the sand grains into a uniform pattern. Work in small, overlapping circles, with light, even pressure, and keep the float flat so the edge does not dig a groove. The motion should match the motion that made the original finish. On most sand finished walls that motion is circular and steady, with no strong direction.

If the float drags or the grains clump, the surface is too dry; mist it lightly and wait a moment. If the mix smears and the grains sink out of sight, the surface is too wet; wait for it to firm up. A fine sand finish can also be closed with a Marshalltown M38 Rubber Float, 9 inches by 4 inches with a fine-cell pad 3/4 inch thick, which gives a slightly tighter surface than a sponge. Whichever float is used, the aim is the same: a flat field of even grain, with the patch edge disappearing into the old work.

Step 8: Blend the edge and protect the cure

The edge of the patch is where the eye goes first, so give it a final pass while the finish is still workable. Dampen a soft brush and draw it lightly along the joint, then follow at once with the float, using the same circular motion and feathering the pressure off as the float crosses onto the old stucco. The goal is a gradual change in texture, not a hard line. Do not overwork the edge; repeated passes pull the sand out of the mix and leave a smooth, shiny band that reads as a scar.

Protect the fresh patch from the weather. Shade it from direct sun for the first day, and keep it damp with a fine mist. The Quikrete premixed patch data sheet notes that the material skins in 20 to 40 minutes and hardens in about 2 hours, with curing continuing for up to 3 days, so the first days matter. Do not paint the patch until the maker guidance allows it: about 2 hours for Rapid Set Stucco Patch before priming and painting, and up to 3 days of cure for the Quikrete premixed patch before a final coating, depending on the coating type. When the patch is painted, use a masonry paint or primer made for stucco, and feather the paint a little beyond the patch so the colour change does not sit exactly on the repair line.

Tools and materials

Quikrete Stucco Patch No. 8650

  • Ready-to-use premixed acrylic patch in a 1 quart pail
  • Sanded formula designed to blend with surrounding stucco texture
  • Repairs cracks, holes, and minor defects up to 1/4 inch thick per layer
  • Coverage about 3.25 square feet at 1/8 inch thick per quart pail
  • Surface skin forms in about 20 to 40 minutes; hard in about 2 hours
  • Curing continues for up to 3 days; apply above 50 degrees Fahrenheit

Quikrete Stucco Patch No. 8650 is the first material to reach for when the damage is shallow. It needs no mixing, which removes the most common source of error on a small repair, and the sanded acrylic formula is made to sit beside an existing sand finish without a visible change in grain. The quart pail suits a patch the size of a hand or a dinner plate; larger damage is better rebuilt with a cement-based material. The 24-hour wait between layers for deeper fills is a real limit, so a hole deeper than 1/4 inch needs either patience or a different product.

Pros: No mixing, ready from the pail; sanded texture suits sand finishes; flexible finish resists hairline cracking.
Cons: Limited to 1/4 inch per layer; quart size suits small patches only; slow full cure before painting.

Rapid Set Stucco Patch

  • Fast-setting cement patch, mixes with water only
  • Working time about 20 minutes at normal temperatures
  • Applied from 1/8 inch to 1 inch thick in a single application
  • Sand is number 16 to 20 silica sand, sized to match common stucco finishes
  • Prime and paint after about 2 hours
  • Mix ratio 1 part water to 4 parts powder; 2 quarts of water per 25 pound bag

Rapid Set Stucco Patch is the structural choice when the hole goes past the finish coat. The 20-minute working time is short, so the wall must be prepared and the tools laid out before the water hits the powder. In exchange, the patch can be built to full depth in one application, which saves a day of waiting between coats on a deep repair. The number 16 to 20 silica sand is the detail that makes this product useful for texture matching: the grain size is close to the aggregate in many sand finish coats, so the floated surface reads as the same finish.

Pros: Full-depth repair in one application; fast return to painting; aggregate sized for texture matching.
Cons: Short working time leaves no room for delay; must be mixed in small batches; stiffens fast in warm weather.

Marshalltown Sponge Float 12 x 5 in

  • High-density sponge pad on a rigid backing plate
  • Pad thickness about 1-1/8 inches
  • Size 12 inches by 5 inches
  • Used for plaster, stucco, concrete, and sand-surface finishing
  • Sponge holds water and keeps the finish damp during floating

The sponge float is the tool that makes a sand finish look like a sand finish. The sponge releases a little water as it moves, which keeps the surface workable and lets the grains roll into a uniform pattern instead of dragging in lines. The 12 by 5 inch size covers a patch in a few passes without being so large that it bridges over hollows. Rinse the sponge often; a sponge loaded with dry mix stops releasing water and starts tearing the surface.

Pros: Even water release for uniform grain; large face covers patches fast; gentle on fresh finish coats.
Cons: Wears faster than a rubber float; needs frequent rinsing; too soft for levelling a brown coat.

Marshalltown M38 Rubber Float Fine 9 x 4 in

  • Sponge rubber pad cemented to an aluminium backing
  • Fine-cell pad for a tight, even surface
  • Size 9 inches by 4 inches; pad thickness 3/4 inch
  • Suited to finishing top coat render and fine sand finishes

The M38 is the float for the final pass when a sponge leaves the surface a touch too open. The fine-cell rubber pad closes the finish a little more, giving a tighter grain that suits walls where the original finish was floated hard. The 9 by 4 inch size is easy to control with one hand and fits into the corners of a patch without touching the old finish around it. Keep the pad clean and slightly damp; a dry rubber float drags and leaves streaks.

Pros: Fine cell gives a tight, even finish; small size suits patch edges; aluminium backing stays flat.
Cons: Less water capacity than a sponge float; can drag if allowed to dry out; not for heavy levelling.

Larsen Weld-Crete Bonding Agent

  • Chemical bonding agent for Portland cement plaster and stucco
  • Bonds new stucco to structurally sound concrete and old stucco
  • Coverage about 200 to 300 square feet per gallon
  • Applied by brush, roller, or spray in a single application
  • Listed to ASTM C1059 for bonding agents

Weld-Crete earns its place on a repair where the substrate is dense or slick and a mechanical key alone cannot be trusted. The maker lists it for bonding Portland cement plaster and stucco mixes to sound concrete, which covers the common case of a patch over an old, hard brown coat. The coverage of 200 to 300 square feet per gallon means a small quantity goes a long way on patch work, and the film can be applied days before the patch in some schedules. The agent is a helper, not a cure: it cannot bond to dust, paint, or loose material, so the cleaning step still comes first.

Pros: Strong chemical bond on dense substrates; wide coverage per gallon; suits stucco and cement plaster.
Cons: No substitute for cleaning and sound preparation; adds a step and a waiting time; see product page for exact timing.

Marshalltown PermaShape Finishing Trowel 14 x 5 in

Marshalltown PermaShape Finishing Trowel 14 x 5 in
  • Stainless steel blade, 14 inches by 5 inches
  • Pre-worn PermaShape edge that limits line and ripple marks
  • Aluminium alloy mounting with a curved DuraSoft handle
  • Blade resists corrosion and cleans easily

The PermaShape trowel is the laying-on tool for the brown and finish coats. The pre-worn edge is the point: a new trowel with a sharp, flat edge leaves lines in fresh plaster, while the broken-in shape of this blade spreads the mix without ridges. The 14 by 5 inch blade is large enough to level a patch in a few passes and small enough to work inside an opening without catching the old edge. Keep the blade clean between passes; dried mix on the edge scores the fresh coat.

Pros: Pre-worn edge limits trowel lines; stainless blade cleans easily; comfortable handle for long sessions.
Cons: Larger blade needs a steady hand on small patches; stainless costs more than carbon steel; see product page for weight.

Common mistakes

Filling a deep hole in one thick layer

A patch thicker than 3/8 inch per coat sets unevenly, shrinks as it dries, and cracks from the inside out. The repair literature is clear on this limit, and every data sheet in the materials list repeats it in some form. Deep holes need layers, with curing time between them. The extra day is cheaper than redoing the patch.

Skipping the sample panel

Texture matching is a matter of hand motion and mix consistency, and neither can be judged from a data sheet. A sample panel on a scrap board takes ten minutes and shows whether the grain, the float pressure, and the timing are right. Skipping it means the first attempt at the finish happens on the wall itself, where a mistake cannot be wiped away.

Patching over wet or dirty stucco

Water behind the stucco and dust on the surface are the two most common causes of a patch that falls off. A patch bonds to whatever it touches, so if it touches dust, it bonds to dust. Clean the opening with a wire brush, blow out the loose material, dampen the surface, and fix the water source before the patch goes on.

Spreading the finish onto the old stucco

A sand finish patch should stop at the edge of the old finish, not overlap it. Spreading new material over old finish leaves a raised lip and a change in grain that the eye catches at once. Tape the edge, keep the finish inside the patch, and feather only the floating motion across the joint, not the material itself.

Painting too soon

Fresh stucco holds moisture, and paint laid over a damp patch can blister or peel. The maker guidance for the products in this guide ranges from about 2 hours before priming for Rapid Set Stucco Patch to up to 3 days of curing for the Quikrete premixed patch. Follow the sheet for the product actually used, and wait longer in cool or damp weather.

Working in hot sun or near freezing

Stucco sets badly at both ends of the temperature range. Hot sun dries the surface before the cement has hydrated, which causes shrinkage cracks; cold weather slows the set and can leave the patch weak. The Quikrete data sheet calls for air and surface temperatures above 50 degrees Fahrenheit, and the FastSet sheet warns against application below 40 degrees or above 100 degrees. Pick a mild, overcast day, and shade the patch while it sets.

FAQ

How thick can a stucco patch be in one coat?

No single coat should exceed 3/8 inch. The scratch and brown coats are each about 3/8 inch thick, and premixed acrylic patches are limited to 1/4 inch per layer, with 24 hours between layers. Deeper holes are rebuilt in layers, and fast-setting cement patches such as Rapid Set Stucco Patch can be applied from 1/8 inch to 1 inch thick in a single application, which is the exception rather than the rule.

How do you match the sand grain of an old finish?

Use a patch material with aggregate in the same size range as the existing finish, and float it with the same tool and motion. Rapid Set Stucco Patch uses number 16 to 20 silica sand, which the maker sizes to match most existing stucco colour coats. A sample panel on a scrap board lets the grain, the mix, and the float motion be settled before the wall is touched.

How long should a scratch coat cure before the brown coat?

Trade guidance calls for moist curing of 48 to 72 hours for the scratch coat, until it is solid but still able to receive the next coat. Mist the surface lightly in dry weather and shade it from direct sun. A scratch coat that dries too fast shrinks and cracks, and those cracks show through the coats above.

Can a premixed patch repair a deep hole?

A premixed acrylic patch suits shallow damage up to 1/4 inch deep per layer. A hole that reaches the brown coat or the lath needs a cement-based patch applied in coats, or a fast-setting product rated for full-depth repair. Using a surface patch for a deep hole leaves a weak repair that cracks and falls away.

Why does a patch show as a different colour?

Fresh stucco dries lighter than old stucco and darkens as it ages and weathers. The colour gap is normal and closes over months, especially once the patch is painted with a masonry coating. A patch that matches in grain and sits flat blends far sooner than a patch that matches in colour on day one but stands proud of the wall.

When can a stucco patch be painted?

It depends on the product. Rapid Set Stucco Patch can be primed and painted after about 2 hours. The Quikrete premixed patch skins in 20 to 40 minutes and hardens in about 2 hours, with curing continuing for up to 3 days, so a final coating should wait until the cure is further along. Always follow the data sheet for the product used, and wait longer in cool or damp weather.

Conclusion

A sand finished exterior wall forgives a lot, but only when the patch is built the way the wall was built. Cut back to sound stucco, undercut the edges, dampen the base, and rebuild in thin coats with curing time between them. Match the sand grain with a material in the same aggregate range, float it with the same circular motion, and stop the finish exactly at the old edge. The products in this guide give the repair its structure: a premixed patch for shallow work, a fast-setting cement patch for deep holes, a sponge float and a fine rubber float for the finish, a bonding agent for dense substrates, and a pre-worn trowel for flat, line-free coats. Done this way, the patch sits quiet beside the old finish, and the wall reads as one surface again.

A
admin88
We compare specs, warranty terms, long-term owner feedback and street pricing before anything earns a spot. Rankings are never paid.
Affiliate disclosure. As an Amazon Associate we earn from qualifying purchases at no extra cost to you. Prices accurate as of the date shown.
Repair Textured Stucco Patches on Sand Finish WallsCheck price on Amazon

Related guides

Browse all How-to, sửa lỗi & học tập guides →

More from Amazon

Programs that pair well with the guide above. Offers and eligibility are set by Amazon and may change.

Amazon Prime

Free shipping on eligible items, Prime Video and more. Eligible new members can start with a free trial.

Start a Prime free trial
Audible

Audiobooks and podcasts to listen to on the go. Eligible new members can start with a free trial.

Try Audible free
Amazon Music Unlimited

Ad-free music streaming. Eligible new subscribers can start with a free trial.

Try Music Unlimited free
Amazon Business

A free business account with business pricing and bulk-buying tools for work, shop or home office.

Create a business account

As an Amazon Associate we earn from qualifying purchases.

Handpicked for this guide

More ways to save on your next finish

Programs that pair well with the guide above. Offers and eligibility are set by Amazon and may change.

Most popular
🏢
Amazon Business
Free to sign up

A free business account with business pricing and bulk-buying tools for work, shop or home office.

Create a business account
🚚
Amazon Prime
Free trial for new members

Fast, free shipping on eligible items, plus Prime Video and more. Eligible new members can start with a free trial.

Start a Prime free trial
📖
Kindle Unlimited
Free trial for new members

Read from a huge library of eBooks, including how-to guides and cookbooks. Eligible new members can start with a free trial.

Try Kindle Unlimited
🎧
Audible
Free trial for new members

Audiobooks and podcasts for the commute, the garage or the kitchen. Eligible new members can start with a free trial.

Try Audible free

As an Amazon Associate we earn from qualifying purchases. Using these links costs you nothing extra.