Updated Th11 26, 2026· 23 min read

Key takeaways

  • Learn how to apply a stucco finish coat over a properly cured basecoat: checks, mixing, trowel work, texture matching, curing, and tools for a lasting result.

As an Amazon Associate I earn from qualifying purchases. This post may contain affiliate links at no extra cost to you.

A stucco finish coat is the thin, visible layer that gives a wall its color, texture, and weather face. The basecoat underneath does the structural work, and the finish coat does the showing work, so the bond between the two layers decides whether the wall looks even for years or starts to map, craze, and shed within a season. How to apply a stucco finish coat over a properly cured compatible basecoat comes down to three things that all have to be right at the same time: a basecoat that has cured long enough and is still sound, a finish mix that matches the basecoat in strength and composition, and an application rhythm that keeps the coat at an even thickness from the first trowel load to the last.

Most finish-coat failures trace back to impatience or to a mismatch between layers. A basecoat that is still green shrinks under the finish coat and pulls it into hairline cracks. A finish coat that is stronger than the basecoat underneath it concentrates stress at the bond line and can delaminate in sheets. A basecoat that has been left too dry sucks the water out of the finish mix before the cement has a chance to hydrate, and the result is a dusty, weak surface that chalks under a fingertip. Each of those problems is avoidable, and none of them requires special equipment. What they require is a clear sequence, a little patience, and a habit of checking the wall before the trowel comes out of the bucket.

This guide walks through that sequence in the order the work actually happens. It starts with how to read a cured basecoat and decide whether it is ready, then covers compatibility between base and finish, mixing, the trowel work itself, texture matching, and the curing routine that follows. The products and materials named in the guide are real, currently sold items with published data sheets, and the figures quoted for coverage, water, and thickness come from those data sheets.

Quick answer

A stucco finish coat goes on a basecoat that has cured for at least 48 hours and, for most cement-based basecoats, a full 7 days is a safer minimum, with the surface sound, clean, and dampened to a uniform dark tone before the mix goes on. The finish coat goes on at about 1/8 inch thick in a single pass, worked with a steel finishing trowel and then floated to the chosen texture while the material is still plastic. Mix only as much as can be placed within the working window of the product, keep the wall out of direct sun and wind while the coat sets, and keep the fresh coat damp for the first 48 hours so the cement hydrates fully. When the basecoat and the finish coat come from compatible cement-based systems and the basecoat has cured properly, the bond is chemical as well as mechanical, and the finish coat becomes part of the wall rather than a skin sitting on top of it.

Item Key specification Best for
SAKRETE Stucco Finish Coat 80 lb bag; about 1.5 gal water per bag; covers about 70 sq ft at 1/8 in. Trowel-applied finish coats on cured basecoats
QUIKRETE Base Coat Stucco No. 1139 80 lb bag; yield about 0.75 cu ft; covers 20 to 24 sq ft at 3/8 in. Scratch and brown basecoats under a finish coat
Marshalltown DuraFlex Finishing Trowel 4681DFDL 13 x 5 in. golden stainless blade; DuraSoft handle; 9 3/4 in. mounting Flexible finishing on smooth and sanded coats
Marshalltown Molded Rubber Float MRF94 9 x 4 in. molded black rubber pad; dense texture; aluminum backing Bringing sand to the surface and evening texture
LaHabra Fastwall 1-Coat Sanded Stucco Base 80 lb bag; about 1.5 gal water; covers 20 to 25 sq ft at 3/8 in. One-coat base work under a compatible finish
Washed sharp sand Clean, washed, angular grains; free of clay and silt Correcting mix workability and matching texture

Step by step

Step 1: Confirm the basecoat has cured

Curing is not the same as drying. A basecoat can look dry on the surface within a day while the cement inside is still hydrating and the coat is still shrinking. The data sheets for cement-based stucco systems put the finish-coat window after the basecoat has had time to cure, and the practical minimum that most manufacturers describe is 48 hours of moist curing before any finish coat goes on, with 7 days as the more conservative figure for a full basecoat system. For a basecoat that was placed in cool or damp weather, the longer end of that range is the right choice, because low temperatures slow hydration and the coat needs more calendar time to reach the same state.

Check the basecoat by looking at it first. The surface should be a uniform color with no dark, damp patches that indicate trapped moisture and no pale, powdery areas that indicate the surface dried too fast. Run a hand across the wall, with a glove on, and feel for hollow spots, loose sand, and soft areas. Tap the surface lightly with a knuckle in several places; a solid, even sound means the coat is bonded, while a hollow drum sound marks a spot that has separated from the substrate and needs to be cut out and re-done before any finish coat goes on. Look for cracks wider than a hairline, and for any crack that runs through the full thickness of the basecoat. Hairline shrinkage cracks in the basecoat are normal and can be bridged by the finish coat, but a wide or moving crack is a sign of a problem underneath that a finish coat cannot fix.

Step 2: Check compatibility between basecoat and finish coat

Compatibility is about strength, composition, and movement. A finish coat should be equal to or weaker than the basecoat beneath it, never stronger, so that stress from temperature change and moisture movement is absorbed by the finish layer rather than concentrated at the bond. Cement-based finish coats belong over cement-based basecoats. Acrylic finishes belong over basecoats that the acrylic manufacturer lists as compatible, and a cement finish coat should not go over an acrylic base that has not been prepared for it. When the basecoat and the finish coat come from the same manufacturer and the same system, compatibility is already established in the system data sheets, and that is the simplest route for a wall that has to last.

Read the finish coat data sheet for the list of approved substrates. The SAKRETE Stucco Finish Coat data sheet, for example, describes a finish coat for use over properly cured, compatible basecoats, and the coverage figures it lists assume a sound, prepared surface. The QUIKRETE Base Coat Stucco No. 1139 data sheet describes a scratch and brown basecoat under ASTM C926, which is the same standard that governs most cement plaster systems, and a finish coat that also meets that standard is a natural match. When the basecoat on the wall is an unknown product, or when it was placed years ago and its composition is uncertain, a small sample panel on an inconspicuous area is the safe move: apply the finish coat to a square foot of the wall, let it cure, and check the bond before committing to the whole wall.

Step 3: Prepare the basecoat surface

Preparation starts with cleaning. Brush the wall with a stiff brush to remove loose sand, dust, and any laitance, which is the thin, weak layer of fine material that can form on the surface of a basecoat. Wash off any dirt, soot, or efflorescence, which is the white salt deposit that sometimes appears on masonry, and let the wall dry to a uniform tone. Efflorescence should be brushed off dry rather than washed, because washing can drive the salts deeper into the pores. Any oil, paint, or sealer on the basecoat has to come off, because a finish coat cannot bond to a sealed surface; a grinder with a wire cup or a chemical stripper made for masonry will take paint and sealer down to sound plaster.

Dampen the basecoat before the finish coat goes on. This is one of the most important steps in the whole job, and it is also one of the most often skipped. A dry basecoat is thirsty, and it pulls water out of the fresh finish mix within minutes, leaving the cement in the finish coat short of the water it needs to hydrate. The result is a finish coat that sets too fast, bonds weakly, and dusts under a hand. Dampen the wall with a fine mist from a pump sprayer until the surface turns a uniform dark tone, then wait a few minutes and check that the surface is damp but not running with water. The wall should look evenly dark, with no dry, pale patches and no standing water in the texture. In hot or windy weather, dampen the wall twice, with a few minutes between passes, so the moisture soaks in rather than flashing off the surface.

Step 4: Mix the finish coat

Mix the finish coat exactly as the data sheet directs, and mix only as much as can be placed before the material starts to stiffen. For the SAKRETE Stucco Finish Coat, the data sheet lists about 1.5 gallons of clean, potable water per 80 lb bag, mixed to a workable, plastic consistency. For the QUIKRETE Finish Coat Stucco No. 1201, the figure is about 2 gallons of water per 80 lb bag, or about 1.25 gallons per 50 lb bag. Those figures are starting points; the exact water demand shifts a little with temperature, humidity, and the moisture content of the sand, so add the water in stages and stop when the mix holds its shape on the trowel without slumping and without tearing.

Use a clean mixing vessel and a paddle mixer on a slow drill, or a mortar mixer for larger batches. Add the water first, then add the dry material while the mixer runs, and mix for two to three minutes until the color is uniform and no dry streaks remain. Let the mix rest for a few minutes so the cement wets out fully, then remix briefly before use. Never add extra water after the mix has started to stiffen, and never retemper a batch that has gone past its working window; a retempered mix loses strength and is the most common cause of a finish coat that dusts and cracks. If the finish coat is a colored product, mix the full quantity for a single wall from the same lot and the same water ratio, because even small changes in water content shift the final color.

Step 5: Apply the finish coat at an even thickness

Load the trowel from the hawk and place the finish coat on the dampened basecoat in a single, even pass at about 1/8 inch thick. Work from the top of the wall downward so that drips and splashes land on work that is still wet and can be blended in, rather than on finished work below. Hold the trowel at a low angle to the wall and push the material on with firm, even pressure, keeping the leading edge of the blade loaded so the coat goes on in a continuous film. The goal at this stage is a coat of uniform thickness with no thin spots and no ridges; texture comes later, and it cannot fix a coat that is thin in one place and thick in another.

Work in manageable sections, and keep a wet edge between sections so the new material blends into the material already on the wall. On a large wall, that means working in vertical strips about four to six feet wide, finishing each strip to texture before moving to the next, and feathering the joint between strips while both sides are still plastic. A finish coat that is allowed to dry at the edge of a section leaves a visible line that no amount of floating will hide. In direct sun or wind, work smaller sections and keep the wall shaded if possible, because a finish coat that dries on the trowel is a finish coat that will crack.

Step 6: Float and texture the coat

Once the coat is on the wall and has firmed up just enough to hold its shape, float it to the chosen texture. For a sand finish, use a rubber float such as the Marshalltown Molded Rubber Float MRF94, which has a molded black rubber pad with a dense texture on an aluminum backing, and work it across the surface in a circular motion with light, even pressure. The rubber face brings the sand in the mix to the surface and evens the texture without tearing the coat. For a smooth finish, use a steel finishing trowel such as the Marshalltown DuraFlex 4681DFDL, with its 13 x 5 inch golden stainless blade, and work the surface with long, overlapping strokes, keeping the blade clean and the pressure even. A flexible blade like the DuraFlex follows the small undulations of the wall and leaves fewer trowel marks than a stiff blade, which matters on a smooth finish where every mark shows.

Match the texture to the wall around the work. On a repair, the texture of the new finish coat has to match the old finish coat, or the patch reads as a different wall. The most reliable way to match is to make a sample panel first: apply the same mix to a small board or an inconspicuous area, float it with the same tool and the same pressure, let it dry, and compare it to the existing wall in daylight. Adjust the float pressure, the timing, or the sand content until the sample matches, then carry those settings to the wall. Texture is set by the tool, the timing, and the mix, and changing any one of them changes the result, so once the sample matches, do not change the routine mid-wall.

Step 7: Cure the finish coat and protect it

Curing is the last step and the one that decides the final strength of the coat. Keep the fresh finish coat damp for the first 48 hours, misting it lightly with a pump sprayer several times a day so the surface never dries out while the cement is hydrating. In hot, dry, or windy weather, mist more often, and consider shading the wall with a tarp or a sheet of plywood set off the surface so air can still move behind it. Protect the coat from freezing for at least 48 hours after it has set, and do not apply a finish coat when the temperature will fall below 40 degrees Fahrenheit within that window, because freezing water inside a fresh coat expands and breaks the bond.

Do not paint, seal, or coat the finish until it has cured. Cement-based finish coats need about 28 days to reach full cure, and that is the figure the LaHabra color coat data sheet gives for its own product. A sealer or a paint applied too early traps moisture in the coat and can cause blistering, peeling, or a color shift. When the coat has cured, check it by running a hand across the surface; it should feel hard and sandy, not dusty or soft, and a light scratch with a fingernail should not remove material. If the surface dusts, the coat was allowed to dry too fast during curing, and the remedy is a fog coat or a penetrating sealer made for the purpose, applied only after the cause has been understood.

Tools and materials

SAKRETE Stucco Finish Coat, 80 lb bag

  • Bag weight: 80 lb
  • Water: about 1.5 gallons per bag, per the product data sheet
  • Coverage: about 70 sq ft at 1/8 inch trowel-applied; about 35 sq ft at 1/4 inch; about 60 sq ft spray-applied at 1/8 inch
  • Colors: gray and white
  • Standard: cement-based finish coat for use over cured, compatible basecoats

The SAKRETE Stucco Finish Coat is a preblended, cement-based finish material that goes on over a properly cured basecoat at about 1/8 inch thick. Its coverage figures show why thickness control matters: the same bag covers about twice the area at 1/8 inch as it does at 1/4 inch, so a coat that runs thick in places wastes material and dries unevenly. The product is available in gray and white, and the white version is the usual choice under a light-colored finish or a fog coat. Mixed to the data sheet water ratio, it holds on the trowel without slumping and spreads in a continuous film, which is what a finish coat has to do if the texture is going to read as one surface.

Pros: Preblended and consistent from bag to bag; coverage figures are published and easy to plan from; gray and white options suit different finish colors.

Cons: Coverage drops sharply if the coat goes on thicker than 1/8 inch; needs a dampened basecoat or the bond suffers; color varies a little from bag to bag, so a single wall should come from one lot.

QUIKRETE Base Coat Stucco No. 1139, 80 lb bag

  • Bag weight: 80 lb
  • Yield: about 0.75 cu ft per bag
  • Coverage: about 20 to 24 sq ft at 3/8 inch; about 15 to 18 sq ft at 1/2 inch
  • Variants: 1139-80 standard, 1139-86 pump grade, 1139-89 with Water-Stop
  • Standard: ASTM C926 base coat stucco

The QUIKRETE Base Coat Stucco No. 1139 is the scratch and brown basecoat that sits under the finish coat in a three-coat system. It is the layer that carries the thickness of the system, and its coverage figures show the difference between the basecoat and the finish coat: a bag of basecoat covers 20 to 24 square feet at 3/8 inch, while a bag of finish coat covers about 70 square feet at 1/8 inch. That difference is the reason the basecoat has to be straight and true before the finish coat goes on, because a finish coat at 1/8 inch cannot hide a basecoat that waves by a quarter inch. The 1139-89 variant includes a water-stop additive for walls that need extra resistance to water entry, and the 1139-86 pump grade is made for machine application.

Pros: Published yield and coverage figures make ordering simple; ASTM C926 compliance matches most finish coat systems; pump grade and water-stop variants cover special cases.

Cons: A bag covers a small area at basecoat thickness, so ordering has to be careful; the basecoat must cure before the finish coat, which adds days to the schedule; not a finish material on its own.

Marshalltown DuraFlex Finishing Trowel 4681DFDL, 13 x 5 in.

  • Blade size: 13 x 5 in.
  • Blade material: golden stainless steel, flexible
  • Handle: DuraSoft rubber grip
  • Mounting: 9 3/4 in.

The Marshalltown DuraFlex 4681DFDL is a flexible finishing trowel with a golden stainless steel blade that bends just enough to follow the small undulations of a wall without digging in. That flexibility is what makes it useful on a finish coat: a stiff blade bridges the low spots and leaves them thin, while a flexible blade keeps contact and lays the material evenly. The DuraSoft handle reduces hand fatigue over a long day of troweling, and the golden stainless blade resists corrosion from the alkaline mix, which keeps the edge clean and the finish free of rust marks. At 13 x 5 inches, the blade covers a good width without being so long that it is hard to control on a small wall or around an opening.

Pros: Flexible blade follows wall undulations and leaves fewer trowel marks; golden stainless steel resists corrosion; DuraSoft handle is comfortable over long sessions.

Cons: A flexible blade is not the right choice for flattening a basecoat; the blade needs cleaning between passes or dried material leaves drag marks; 13 inches can feel long in tight corners.

Marshalltown Molded Rubber Float MRF94, 9 x 4 in.

  • Pad size: 9 x 4 in.
  • Pad material: molded black rubber, dense texture
  • Backing: lightweight aluminum, permanently cemented to the pad
  • Use: bringing sand to the surface; used by concrete finishers, plasterers, and tile setters

The Marshalltown Molded Rubber Float MRF94 is a rubber float with a molded black rubber pad that has a dense texture, bonded to a lightweight aluminum backing. Its job on a finish coat is to bring the sand in the mix to the surface and to even out the texture after the steel trowel has laid the material. The dense texture of the pad grips the fresh coat just enough to move the sand without tearing the surface, and the aluminum backing keeps the pad flat so the pressure stays even across the whole face. At 9 x 4 inches, it is small enough to work around windows, corners, and piers, and it is the right size for blending a finish coat into an existing texture.

Pros: Dense rubber face evens sand texture without tearing; aluminum backing keeps the pad flat; size suits detail work and blending.

Cons: A rubber float cannot produce a smooth, steel-troweled finish on its own; the pad wears with use and needs replacement when the texture goes uneven; needs a damp surface or it drags.

LaHabra Fastwall 1-Coat Sanded Stucco Base, 80 lb bag

  • Bag weight: 80 lb
  • Water: about 1.5 gallons per bag
  • Coverage: about 20 to 25 sq ft at 3/8 inch; about 15 to 19 sq ft at 1/2 inch
  • Minimum application temperature: 40 degrees Fahrenheit
  • Set time: 30 to 45 minutes
  • Shelf life: 15 months

The LaHabra Fastwall 1-Coat Sanded Stucco Base is a one-coat base material that goes on as the base layer under a compatible finish coat. Its data sheet lists a set time of 30 to 45 minutes, which sets the working window for the crew: the material has to be placed, rodded, and floated within that window, and the finish coat cannot go on until the base has cured. The coverage figures, 20 to 25 square feet at 3/8 inch, are in the same range as other cement basecoats, and the 40 degree minimum application temperature is the standard limit for cement plaster work. A 15 month shelf life means the bag can be stored between jobs, provided it stays dry.

Pros: One-coat base simplifies the system; published set time and coverage make scheduling straightforward; 15 month shelf life is generous.

Cons: A 30 to 45 minute set time leaves little room for delay; needs the same curing wait as any basecoat before the finish coat; minimum 40 degree application temperature limits cold-weather work.

Washed sharp sand

  • Type: clean, washed sand with angular grains
  • Contamination: free of clay, silt, and organic matter
  • Use: adjusting mix workability and matching finish texture
  • Source: masonry supply or building materials dealer

Washed sharp sand is the plainest item on the list and one of the most important. Sharp sand has angular grains that lock together in the mix, while rounded river sand rolls and makes a mix that is harder to hold on the trowel. Washing removes clay and silt, which weaken the bond and cause the finish coat to dust, and it removes organic matter, which can stain the finish. On a finish coat, a small addition of sharp sand can open up a mix that is too tight and help the texture match an existing wall, but the addition has to be measured and consistent, because sand content is one of the things that changes the final color and texture. The right habit is to buy washed sharp sand from a masonry supplier, keep it covered and dry, and add it by the bucket, not by the shovelful, so the ratio stays the same from one batch to the next.

Pros: Inexpensive and widely available; angular grains improve the mix; washing removes the contaminants that weaken a finish coat.

Cons: Quality varies by supplier, so the sand has to be checked; unwashed sand causes dusting and staining; adding sand by eye changes color and texture from batch to batch.

Common mistakes

Putting the finish coat on a green basecoat

A basecoat that has not cured is still shrinking, and a finish coat placed over it is pulled into hairline cracks as the basecoat moves underneath. The fix is calendar time: wait at least 48 hours, and 7 days for a full basecoat system, before the finish coat goes on. When the schedule is tight, the temptation is to start early, and the cost of starting early is a finish coat that cracks in the first month. A basecoat that has cured properly is hard, uniform in color, and silent when tapped.

Skipping the dampening step

A dry basecoat pulls water out of the fresh finish mix in minutes, and the finish coat sets before the cement has hydrated. The surface ends up weak, dusty, and poorly bonded. Dampen the wall with a fine mist until it turns a uniform dark tone, wait a few minutes, and dampen again if dry patches appear. The wall should be damp, not running with water, when the first trowel load goes on.

Mixing the finish coat too wet

Extra water makes a mix that is easy to spread and hard to keep on the wall. A wet mix shrinks more as it dries, which causes crazing, and the extra water carries the fine cement to the surface, where it forms a weak, dusty skin. Mix to the data sheet water ratio, add water in stages, and stop when the mix holds its shape on the trowel. A mix that slumps off the trowel is too wet, and a mix that tears as it is spread is too dry.

Letting the coat dry at the edge of a section

A finish coat that dries at the edge of a work section leaves a line that cannot be floated out. Work in vertical strips, keep a wet edge between strips, and finish each strip to texture before moving on. On a large wall, that means planning the sequence before the first batch is mixed, so the crew knows where each strip starts and ends and no one is left holding a trowel at a dry joint.

Floating the texture too early or too late

Floating too early tears the surface and pulls the sand out of the mix. Floating too late means the coat has already started to set, and the float leaves drag marks and a patchy texture. The right moment is when the coat has firmed up enough to hold its shape but is still plastic under the float. That window is usually a matter of minutes, and it shortens in sun and wind, so the crew has to watch the wall rather than the clock.

Sealing or painting before the coat has cured

A finish coat needs about 28 days to cure fully. A sealer or a paint applied in the first days traps moisture in the coat and can cause blistering, peeling, or a color shift that shows as a pale patch. Wait for the full cure, check the surface by hand, and only then apply a finish sealer or a paint that the manufacturer lists as compatible with a cured cement finish.

FAQ

How long should a basecoat cure before the finish coat goes on?

A cement basecoat should cure for at least 48 hours before a finish coat goes on, and 7 days is the more conservative figure for a full scratch and brown system. The basecoat should be hard, uniform in color, and sound when tapped, with no hollow spots and no wide cracks. In cool or damp weather, the longer end of the range is the right choice, because low temperatures slow hydration and the coat needs more calendar time to reach the same state.

What happens if the finish coat goes on too thick?

A finish coat is meant to go on at about 1/8 inch thick. At 1/4 inch, the same bag covers about half the area, the coat dries unevenly, and the thicker sections shrink more and are more likely to craze. A thick coat also adds weight that the bond has to carry. When the basecoat is out of true, the right move is to straighten the basecoat, not to bury the problem under a thick finish coat.

Can a finish coat go over an old, painted stucco wall?

A finish coat cannot bond to paint, sealer, or any other coating that seals the surface. The old coating has to come off, down to sound plaster, before the finish coat goes on. A grinder with a wire cup, a chemical stripper made for masonry, or a combination of the two will take paint and sealer off. After stripping, the wall has to be cleaned, checked for soundness, and dampened in the same way as a new basecoat.

How does the finish coat get the same texture as the old wall?

Texture is set by the tool, the timing, and the mix. Make a sample panel first, using the same mix, the same float, and the same pressure as the planned work, and let it dry before comparing it to the old wall in daylight. Adjust the float pressure, the timing, or the sand content until the sample matches, then carry those settings to the wall without changing them. A rubber float such as the MRF94 brings sand to the surface for a sand finish, while a steel trowel such as the DuraFlex 4681DFDL gives a smooth finish.

How long does a finish coat take to cure?

A cement-based finish coat takes about 28 days to reach full cure, and that is the figure the LaHabra color coat data sheet gives for its own product. The coat should be kept damp for the first 48 hours, protected from freezing for at least 48 hours after it sets, and left unpainted and unsealed until the full cure is complete. A coat that has cured properly feels hard and sandy under a hand, and a light scratch with a fingernail does not remove material.

Conclusion

A stucco finish coat over a properly cured, compatible basecoat is a straightforward job when the sequence is respected: cure the basecoat, check compatibility, clean and dampen the surface, mix to the data sheet, place the coat at an even 1/8 inch, float it to the chosen texture, and keep it damp during curing. Each step is simple on its own, and the failures that show up on stucco walls almost always come from skipping one of them. The basecoat is the foundation, the finish coat is the face, and the bond between them is what makes the wall last. Give the basecoat its curing time, keep the mix at the right water ratio, and let the coat cure before it is sealed or painted, and the finish will read as one even surface for years.

A
admin88
We compare specs, warranty terms, long-term owner feedback and street pricing before anything earns a spot. Rankings are never paid.
Affiliate disclosure. As an Amazon Associate we earn from qualifying purchases at no extra cost to you. Prices accurate as of the date shown.

Related guides

Browse all How-to, sửa lỗi & học tập guides →

Handpicked for this guide

More ways to save on your next finish

Programs that pair well with the guide above. Offers and eligibility are set by Amazon and may change.

Most popular
🏢
Amazon Business
Free to sign up

A free business account with business pricing and bulk-buying tools for work, shop or home office.

Create a business account
🚚
Amazon Prime
Free trial for new members

Fast, free shipping on eligible items, plus Prime Video and more. Eligible new members can start with a free trial.

Start a Prime free trial
📖
Kindle Unlimited
Free trial for new members

Read from a huge library of eBooks, including how-to guides and cookbooks. Eligible new members can start with a free trial.

Try Kindle Unlimited
🎧
Audible
Free trial for new members

Audiobooks and podcasts for the commute, the garage or the kitchen. Eligible new members can start with a free trial.

Try Audible free