A soap treated sample board is a small, flat, forgiving surface, and a repair on it takes far less time than the same repair on a full wall. How long does it take to repair minor marks in tadelakt on a soap treated sample board has two answers, and both matter. The hands on work takes a few hours spread across a day: cleaning, mixing, laying the patch, closing it, and burnishing it with a stone. The full sequence takes much longer, because the plaster needs time to dry, the soap needs time to react with the lime, and the wax needs a dry cured surface before it goes on. A board that is rushed back into use will show it, while a board given its drying time will carry a repair that disappears into the surface.
The board in this guide is a sample board of about half a square metre, finished with tadelakt and treated with soap, with a few minor marks: a scuff, a shallow scratch, a dull patch where the soap has worn thin, and a small chip at one corner. The repair uses artSparx Tadelakt Moroccan Lime Plaster, because the maker lists clear drying times for it, and the soap, stone, and wax in the list are the materials that finish the repair. Where a time comes from the maker, it is given as listed. Where a time depends on the room, it is given as a range, with the conditions that stretch it or shorten it.
This guide walks through the sequence with the clock in mind, so each step can be planned around the drying gaps rather than fought against them.
Quick answer
The hands on work of repairing minor marks in tadelakt on a soap treated sample board takes about two to three hours spread across a day: roughly half an hour to clean and prepare the marks, half an hour to mix and lay the patch, and an hour or so of closing, burnishing, and soaping as the plaster firms. The patch then needs at least a day to dry before the colour can be judged, and the soap coat can be repeated after 2 to 3 days. The wax coat needs a fully dry cured surface, and the surface reaches its full hardness after about 4 weeks, with the plaster stable at 180 days. In practice, the board can be handled normally after a day, and the repair is fully finished once the wax has been applied and buffed.
| Item | What it does | When to use it |
|---|---|---|
| artSparx Tadelakt Moroccan Lime Plaster | Supplies the patch plaster for the board | For every fill, from a hairline scratch to a shallow chip |
| artSparx Standard Colours #1–12 | Matches the colour of the patch to the board | When the board was tinted and the patch needs the same tone |
| Kreidezeit Tadelakt Polishing Stone ST177 | Burnishes the patch and closes the pores | While the patch still holds moisture |
| Galtane Polishing Soap 2035 | Re-seals the repair and restores the finish | After the patch has dried, and again after 2 to 3 days |
| Granite polishing stone | Compresses the patch and gives it a shine | While the patch still holds moisture, in small circles |
| Kreidezeit Carnauba Wax Emulsion | Seals the repair with a wax finish | Once the area is completely dry |
Step by step
1. Read the marks and plan the day (about 15 minutes)
Hold the board under a raking light and look at each mark from several angles. A surface scuff that has not broken the plaster needs only soap and stone, and it takes minutes. A shallow scratch that catches a fingernail needs a thin fill, and it takes an hour or so including the drying gap. A chip with a raised edge needs the loose edge cut away first, and it takes a little longer. A dull patch where the soap has worn thin needs soap alone. Sorting the marks into these groups decides how much of the day the repair will take, and it keeps a small job small. Note the colour of the board around each mark as well, because a tinted board needs a tinted patch, and the pigment for that patch should be weighed out before any plaster is mixed.
2. Clean the board and dampen the repair zones (about 15 minutes)
Wipe the board with a soft cloth barely dampened with clean water, and pick up any dust from the marks with a soft brush. Cut away any loose plaster with a sharp craft knife, working from the outside of the damage toward the centre, and open shallow scratches slightly so the patch can key into them. Brush away every crumb. Dampen each repair zone lightly and let it sit for a few minutes while the materials are laid out, so the surface is evenly damp rather than wet in one place and dry in another. The cleaning and preparation take about 15 minutes for a board with a handful of marks, and the dampening needs a few minutes more before the patch goes on.
3. Mix the patch plaster (about 10 minutes of work, plus a rest)
Weigh out a small amount of artSparx Tadelakt Moroccan Lime Plaster, about 50 grams for a mark the size of a coin, and add water at about 32 percent by weight of powder, which is the dilution the maker lists. Stir the pigment paste into the mixing water first if the board was tinted, using one of the artSparx Standard Colours, then add the powder and mix thoroughly. The maker lists the mixture as best used between 4 hours and 24 days from preparation, so a batch mixed in the morning stays usable for the whole day and far beyond, which takes the time pressure off the repair. Mix only as much as the marks need, because a patch mixed too wet will shrink and crack as it dries, while a patch mixed too dry will drag and leave a rough surface.
4. Lay the patch in thin layers (about 30 minutes)
Press the paste into each mark with a small spatula, working from the edges toward the centre so no air is trapped, and keep each layer thin, no more than a millimetre or two. Let the first layer lose its wet shine before adding a second layer if a hollow is deep, and feather the edges onto the sound plaster around each mark. The laying takes about half an hour for a board with a handful of marks, including the short wait between layers. Wipe away any plaster that has spread beyond the repair zones with a damp cloth before it starts to set, because dried smears on a soaped surface are hard to remove without scratching the finish.
5. Close the patch and burnish it with the stones (about 45 minutes)
Once the patch has lost its wet shine, close the surface with a plastic trowel, passing over each repair in several directions to close the small holes and pores. Then take the Kreidezeit Tadelakt Polishing Stone ST177 and rub it over the patch in small circles, starting with very little pressure and increasing it slowly as the surface firms. The stone is hardened ceramic with a hardness grade of 9.5 Mohs, pore free and ergonomically shaped, and it is used by hand with polishing soap in small circular motions. Follow with the granite polishing stone, which is a hard fine grained stone with a flat face and rounded edges, and work each patch until the surface shines where the stone has passed. If a stone picks up plaster, the patch is still too wet, so wait a little longer and check again. The closing and burnishing take about 45 minutes for a board with several marks, with short waits while each patch firms.
6. Let the patch dry and judge the colour (at least 1 day)
Leave the board alone for at least a day before judging the repair. The maker lists the artSparx plaster as carbonating to the touch in about 3 hours at 20 degrees, and below the surface in about 48 hours, so the surface may feel dry within hours while the plaster below is still hardening. The general guidance for tadelakt puts touch dry at under 24 hours, and full hardening at approximately 4 weeks, with the artSparx plaster stable at 180 days. Wet lime always looks darker than dry lime, so a patch that looks like a perfect match while wet will often dry paler than the board. Judge the colour under the same light as the rest of the board, and only after a full day of drying.
7. Re-soap the repair (about 20 minutes, plus drying)
When the patch has dried, brush Galtane Polishing Soap 2035 over the repair with a brush until the surface is saturated, let it set a little, then polish it with the stone. The soap creates a deeper shine and better resistance to water and dirt, because the chemical reaction of the soap with the lime in the plaster provides the water repellent quality. The maker guidance calls for a second coat of polishing soap after 2 to 3 days to increase the water resistance further. Each soap coat takes about 20 minutes of work, plus the drying time, and the board should be left alone between coats. The plaster is recoatable after 12 to 20 hours at 68 degrees Fahrenheit, so the soap coats fit comfortably into a schedule of a day apart.
8. Wax the repair once the surface is completely dry (about 30 minutes)
Finish with Kreidezeit Carnauba Wax Emulsion once the area is completely dry. The wax is water based and is easily applied with a brush, sponge, or soft cloth, and a higher sheen comes from buffing with a lambswool bonnet on a polishing machine. Brush or wipe the wax on in a thin coat, let it dry, and buff it to a shine. The wax coat takes about half an hour of work. After the wax, the board should be left to harden, and the surface reaches its full hardness after about 4 weeks. A useful habit from the application guidance is to re-soap the whole surface one week after completion, and to re-soap every 1 to 2 months, which keeps the finish fresh and the water repellent skin intact.
Tools and materials
artSparx Tadelakt Moroccan Lime Plaster
- Lime based plaster, marble dust, fine marble aggregate, slaked aged lime
- 18 kg covers 75 to 100 square feet, 1,700 to 2,200 grams per square metre
- Dilution about 32 percent water by weight of powder
- Use between 4 hours and 24 days from preparation
- Carbonation 3 hours to the touch at 20 degrees, 48 hours below the surface, stable 180 days
- 20 kg bucket, particle stones 0.8 mm, white, can be tinted
artSparx Tadelakt Moroccan Lime Plaster is the patch plaster for this board repair, and it is chosen because the maker lists clear drying times for it. The plaster is a blend of marble dust, fine marble aggregate, slaked aged lime, and other materials, and an 18 kg bucket covers 75 to 100 square feet, which is 1,700 to 2,200 grams per square metre. The maker lists a dilution of about 32 percent water by weight of powder, use between 4 hours and 24 days from preparation, carbonation in 3 hours to the touch at 20 degrees, 48 hours below the surface, and stability at 180 days. The long usable window after mixing takes the time pressure off the repair, because a batch mixed in the morning stays workable for the whole day.
Pros: Long usable window after mixing, so the repair can be paced without rushing; clear drying times from the maker.
Cons: Full hardness takes about 4 weeks, so the board needs gentle handling for a while after the repair.
artSparx Standard Colours #1–12
- Mineral colours for tinting artSparx Tadelakt
- 20 ml bottles, standard tones 1 to 12
- Stir into the mixing water before the powder goes in
- Allows a patch to match a tinted board
artSparx Standard Colours are the colour matching material for a tinted board. The colours come in 20 ml bottles, in standard tones 1 to 12, and they are stirred into the mixing water before the powder goes in, so the colour is even through the batch. A patch mixed without colour on a tinted board will show as a pale island, while a patch mixed with the right tone will disappear once it has dried. Weigh or measure the colour rather than guessing, and keep a note of the amount so the same tone can be mixed again if the repair needs a second layer.
Pros: Allows a patch to match a tinted board closely; small bottles suit the tiny quantities a sample board needs.
Cons: Colour looks darker while the patch is wet, so matching by eye during mixing is unreliable without a measured amount.
Kreidezeit Tadelakt Polishing Stone ST177
- Hardened ceramic polishing stone, hardness grade 9.5 Mohs
- Pore free, ergonomically shaped
- Used by hand with Polishing Soap in small circular motions
- Closes the pores and gives the patch its shine
The Kreidezeit Tadelakt Polishing Stone ST177 is the first burnishing tool for this repair. The stone is hardened ceramic with a hardness grade of 9.5 Mohs, pore free and ergonomically shaped, and it is used by hand with polishing soap in small circular motions. The stone is used while the patch still holds moisture, pressing the aggregate together and closing the pores, and the shine that appears under the stone shows where the surface has closed. Because the stone is far harder than the plaster, it compresses the surface rather than scratching it.
Pros: Very hard face closes the patch without scratching; ergonomic shape suits work by hand.
Cons: Needs the patch at the right dampness, and a stone used too hard too soon will pick up plaster.
Galtane Polishing Soap 2035
- Polishing soap for Galtane Tadelakt, reference 2035
- Apply with a brush until the surface is saturated
- Let it set a little before polishing with the stone
- Second coat after 2 to 3 days to increase water resistance
- Recoatable after 12 to 20 hours at 68 degrees Fahrenheit
Galtane Polishing Soap 2035 is the re-soaping material for this repair. The soap is applied with a brush until the surface is saturated, left to set a little, and then polished with the stone, which creates a deeper shine and better resistance to water and dirt. The maker guidance calls for a second coat after 2 to 3 days to increase the water resistance further, and the plaster is recoatable after 12 to 20 hours at 68 degrees Fahrenheit, so the soap coats fit into a schedule of a day apart. The chemical reaction of the soap with the lime in the plaster is what builds the water repellent quality of the finish.
Pros: Two coats build a strong water repellent skin; the timing fits a schedule of a day apart.
Cons: Needs a second coat after 2 to 3 days, so the repair spans several days.
Granite polishing stone
- Hard fine grained stone, granite, basalt, or agate
- Flat face with rounded edges, shaped into oval forms
- Used by hand in small circles while the patch still holds moisture
- Listed as a suitable polishing stone for tadelakt
The granite polishing stone is the second burnishing tool for this repair. Granite is a hard fine grained stone, and the maker guidance lists granite, basalt, and agate as suitable polishing stones, with a flat face and rounded edges shaped into oval forms. The stone is used by hand in small circles while the patch still holds moisture, following the first pass with the ceramic stone, and it gives the patch its final shine. Two stones with slightly different faces can catch small hollows that one stone alone might miss, and the granite stone is a natural complement to the ceramic stone.
Pros: Hard flat face gives a final shine; rounded edges follow the board without digging in.
Cons: Needs the patch at the right dampness, like any stone, and it works best as a second pass rather than the first.
Kreidezeit Carnauba Wax Emulsion
- Water based wax emulsion for tadelakt
- Applied with a brush, sponge, or soft cloth once the area is completely dry
- Higher sheen when buffed with a lambswool bonnet on a polishing machine
- Seals the repair and protects the finish
Kreidezeit Carnauba Wax Emulsion is the sealing finish for this repair. The wax is water based and is easily applied with a brush, sponge, or soft cloth once the area is completely dry, and a higher sheen comes from buffing with a lambswool bonnet on a polishing machine. The wax goes on only when the surface is completely dry, because moisture under the wax will cause spots, and it should be applied in a thin coat and buffed to a shine. The wax adds a layer of protection over the soap skin, and it can be renewed later to keep the finish fresh.
Pros: Water based and easy to apply; buffing gives a higher sheen on the repair.
Cons: Needs a completely dry surface, so it cannot go on until the patch has cured.
Common mistakes
Judging the repair too soon
A patch that feels dry to the touch within hours is still hardening below the surface, and the colour will keep changing as it dries. The maker lists carbonation in 3 hours to the touch and 48 hours below the surface, with full hardness at about 4 weeks, so a repair judged after an hour will always look wrong. Wait at least a day before judging the colour, and a week before judging the finish.
Waxing before the surface is completely dry
The wax should go on only when the area is completely dry, because moisture under the wax will cause spots that are hard to remove. A patch waxed too soon can show pale spots where the moisture was trapped. Let the patch dry for a day, re-soap it, and wait for the curing period before the wax goes on.
Skipping the second soap coat
The first soap coat builds the water repellent skin, and the second coat after 2 to 3 days increases the water resistance further. A repair with only one soap coat will look finished but will wear faster than the board around it. Brush the second coat on after the first has dried, polish it with the stone, and let it dry before the wax goes on.
Pressing the stone too hard too soon
A stone pressed hard into a wet patch will pick up plaster and leave a hollow, while a stone used gently in small circles will close the surface. Start with very little pressure, and increase it only as the surface firms. If plaster comes off on the stone, wait a little longer and check again before continuing.
Mixing the patch too wet
A wet mix is easy to spread, but it shrinks as it dries and can crack across the repair. Add water a little at a time, aiming for the listed dilution of about 32 percent water by weight of powder, and aim for a paste that holds its shape on the trowel. A patch mixed to the right stiffness dries with far less shrinkage and needs no second fill.
Handling the board before it has hardened
The surface may feel dry within hours, but the plaster below is still hardening, and the soap needs time to react with the lime. A board handled roughly in the first day can pick up fingerprints and smudges on the soft repair. Leave the board flat and untouched for a day after the soap coat, and handle it gently for the first week while it hardens.
FAQ
How long does the hands on work take?
About two to three hours spread across a day: roughly half an hour to clean and prepare the marks, half an hour to mix and lay the patch, and an hour or so of closing, burnishing, and soaping as the plaster firms. The waits between steps are part of the work, because each layer needs to lose its wet shine before the next step, and the stone work needs the patch at the right dampness.
When can the board be handled normally?
The board can be handled gently after a day, once the patch has dried and the first soap coat has been applied and polished. The surface may feel dry to the touch within hours, but the plaster below the surface is still hardening, and the soap needs time to react with the lime. Full hardness takes about 4 weeks, so the board should be handled gently for the first week and kept dry while the finish hardens.
How long should the repair dry before the wax goes on?
The wax should go on only when the area is completely dry, and the plaster needs time to cure first. The patch should dry for at least a day, the soap coats should be applied and left to dry, and the surface should be fully dry before the wax. A useful rhythm is to patch on day one, soap on day two, soap again after 2 to 3 days, and wax once the surface is completely dry, which is usually within the first week.
How long does a mixed batch of plaster stay usable?
The maker lists the artSparx mixture as best used between 4 hours and 24 days from preparation, so a batch mixed in the morning stays usable for the whole day and far beyond. That long window takes the time pressure off the repair, because the patch can be laid, closed, and burnished without rushing. Keep the mixed plaster covered between uses so it does not dry out on the surface.
What should be done if the patch dries a different colour from the board?
First check whether the patch is fully dry, because a damp patch always looks darker, and the colour keeps changing for a day or two as the plaster carbonates. If the patch is dry and still too pale, mix a second thin layer with a little more colour and lay it over the first, then close it with the trowel and stone it again. If the patch is too dark, a thin layer of untinted plaster over the top can lighten it.
How often should the board be re-soaped after the repair?
The application guidance calls for re-soaping the whole surface one week after completion, and re-soaping every 1 to 2 months after that. The soap keeps the water repellent skin fresh, and a board that is re-soaped on that rhythm will hold its shine and its protection far longer than a board that is left alone. Each re-soap takes only a few minutes on a sample board.
Conclusion
A tadelakt repair on a soap treated sample board takes about two to three hours of hands on work spread across a day, and about a week from the first cleaning to the final wax coat. The patch itself is quick: clean the marks, mix a small batch of artSparx plaster at about 32 percent water by weight, lay it thin, close it with a trowel, and burnish it with the ceramic and granite stones while it still holds moisture. The waiting is the longer part: a day for the patch to dry, a second soap coat after 2 to 3 days, and a wax coat once the surface is completely dry, with full hardness at about 4 weeks and stability at 180 days. Give the board that time, re-soap it a week after completion and every month or two after that, and the repair will sit flush with the board, match it in colour and shine, and carry the same water repellent skin as the rest of the surface.
Related guides
More ways to save on your next finish
Programs that pair well with the guide above. Offers and eligibility are set by Amazon and may change.
A free business account with business pricing and bulk-buying tools for work, shop or home office.
Create a business accountFast, free shipping on eligible items, plus Prime Video and more. Eligible new members can start with a free trial.
Start a Prime free trialRead from a huge library of eBooks, including how-to guides and cookbooks. Eligible new members can start with a free trial.
Try Kindle UnlimitedAudiobooks and podcasts for the commute, the garage or the kitchen. Eligible new members can start with a free trial.
Try Audible freeAs an Amazon Associate we earn from qualifying purchases. Using these links costs you nothing extra.
Write Your Review
No reviews yet. Be the first to share your experience!